Applylabwork Mpt-sp001pk Msla Spring Pink Instructions

Applylabwork Mpt-sp001pk Msla Spring Pink Instructions

ApplyLabWork-LOGO

ApplyLabWork MPT-SP001PK MSLA Spring Pink

ApplyLabWork-MPT-SP001PK-MSLA-Spring-P-PRODUCT

Check

  • Resin tank and LCD screen are clean
  • Shake resin bottle well before use
  • Tank and plateform are properly fastened

Printer Settings Recommendation

BrandModelLayer height

(mm)

Bottom Layer

counts

Exposure time

(s)

Bottom Exposure

(s)

Lifting Speed

(mm/min)

Lifting Distance

(mm)

Retract Speed

(mm/min)

PhrozenSonic0.16430608120
Sonic mini0.165.530608120
Sonic Mighty 4 K0.110460608120
ElegooMars2 Pro0.163.630608120
Mars30.163.630608120
  Layer height

(mm)

Bottom Layer

counts

Exposure time

(s)

Bottom Exposure

(s)

Lifting Speed

(mm/s)

Lifting Distance

(mm)

Retract Speed

(mm/s)

AnycubicMonoX0.162.230182
  • Light-off Delay = 15s under current lift-retract motion. [ When printing large object, increase Lifting Distance and recalculate Light-off Delay ]
  • For Sonic Mighty 4K, please set Transition Layer Count to 20
  • Light intensity varies each printer. Please adjust exposure time ±0.1~0.5 second and/or XY dimesion ratio according to printing result and part application.

Parts Recommendation

  • Avoid large aspect-ratio geometry (e.g. thin wall or long thin rod) in the sturcture to reduce failures.
  • If support is needed, please set contact diameter>1.2(mm), and density>60%

Washing

Wipe off excess resin on printed parts with paper towel, submerge into 95% IPA and place the container in ultrasonic bath, wash for 5 minutes. Replace by clean IPA and repeat ultrasonic washing for another 5 mintes (total 10 minutes). Blow off all excess IPA and set parts in a shaded, ventilated place to dry at least 2 hours before curing. Dried print will be tacky to touch

Post-curing (Mandatory)

Submerge the parts into glycerol/glycerin(CAS # 56-81-5) and start FormCure with 60 ℃ / 30 mins setting. Wash off glycerol in water and dry off with paper towel.

  • If prints don’t sink completely into glycerol, add water (no more than half of volume) to adjust liquid density.
  • If prints are still tacky to touch after post-curing, rinse with acetone (CAS # 67-64-1) for no more than 1 minute will significantly reduce tackiness

Storage

  • Keep resin away from heat and light.
  • NOT accessible to children

Note:

  • Keep printing environment well ventilated.
  • Wear gloves when handling Spring resin and avoid direct contact.
  • Vibration of the parts during printing process might cause resin splash onto printer ’s cover. Use paper towel and IPA to clean immediately.
  • Slight pigment settlement is normal.Gentally mix remaining resin in resin tank with rubber spetula for color evenness.
  • Don’t leave the parts on building platform after printing for more than one day.
  • Color of printed parts will gradually turn yellow if contiuously receive photon energy.
  • Spring resin should NOT use with food, drink, or on/in the human body unless specifically indicated.

Prototype Engineering Series